Solution
The entire process from concentration to deep dewatering of lead-zinc tailings
Step 1 (Concentration):The DNY type concentration dewatering integrated machine increases the tailings slurry concentration from 15% to 40%, reducing the subsequent filtration load;;
Step 2 (Main Dehydration):The DU type rubber belt vacuum filter continuously dehydrates, reducing the moisture content of the filter cake to 20% and meeting the requirements for dry stacking.;
Step 3 (Deep Drying):If further reduction of moisture content is required (such as for building materials), connect the DZY type press vacuum filter to achieve a final moisture content of 18%..